Dancolor
TPU colour masterbatches (aromatic / aliphatic)
For extrusion, injection moulding and calender application.
Many special colours available on request, for customer-specific applications.
Please contact us for detailed technical information.
DANCOLOR MB
Colour Masterbatches (aromatic TPU matrix)
Product name
Description
Data sheet
Safety data sheet
Polymer
Thermoplastic polyurethane
Processing
Dosage: 1- 3 %
Chemical structure
Aromatic
Form of delivery
Granules
Processing conditions
Max.: 205°C
Polymer
Thermoplastic polyurethane
Processing
Dosage: 3 %
Chemical structure
Aromatic
Form of delivery
Granules
Processing conditions
Max.: 215°C
Polymer
Thermoplastic polyurethane
Processing
Dosage: 1- 3 %
Chemical structure
Aromatic
Form of delivery
Granules
Processing conditions
Max.: 215°C
Polymer
Thermoplastic polyurethane
Processing
Dosage: 2 %
Chemical structure
Aromatic
Form of delivery
Granules
Processing conditions
Max.: 215°C
Polymer
Thermoplastic polyurethane
Processing
Dosage: 2 %
Chemical structure
Aromatic
Form of delivery
Granules
Processing conditions
Max.: 215°C
Polymer
Thermoplastic polyurethane
Processing
Dosage: 1- 3 %
Chemical structure
Aromatic
Form of delivery
Granules
Processing conditions
Max.: 215°C
Polymer
Thermoplastic polyurethane
Processing
Dosage: 1- 2 %
Chemical structure
Aromatic
Form of delivery
Granules
Processing conditions
Max.: 240°C
Polymer
Thermoplastic polyurethane
Processing
Dosage: 1- 4 %
Chemical structure
Aromatic
Form of delivery
Granules
Processing conditions
Max.: 215°C
Polymer
Thermoplastic polyurethane
Processing
Dosage: 1-3 %
Chemical structure
Aromatic
Form of delivery
Granules
Processing conditions
Max.: 240°C
Polymer
Thermoplastic polyurethane
Processing
Dosage: 1- 3 %
Chemical structure
Aromatic
Form of delivery
Granules
Processing conditions
Max.: 240°C
Polymer
Thermoplastischic polyurethane
Processing
Dosage: 1- 3 %
Chemical structure
Aromatic
Form of delivery
Granules
Processing conditions
Max.: 240°C
Polymer
Thermoplastic polyurethane
Processing
Dosage: 1- 3 %
Chemical structure
Aromatic
Form of delivery
Granules
Processing conditions
Max.: 240°C
Polymer
Thermoplastic polyurethane
Processing
Dosage: 3 %
Chemical structure
Aromatic
Form of delivery
Granules
Processing conditions
Max.: 215°C
Polymer
Thermoplastic polyurethane
Processing
Dosage: 1- 10 %
Chemical structure
Aromatic
Form of delivery
Granules
Processing conditions
Max.: 205°C
Polymer
Thermoplastic polyurethane
Processing
Dosage: 2- 4 %
Chemical structure
Aromatic
Form of delivery
Granules
Processing conditions
Max.: 190°C
Polymer
Thermoplastic polyurethane
Processing
Dosage: 1- 5 %
Chemical structure
Aromatic
Form of delivery
Granules
Processing conditions
Max.: 205°C
Polymer
Thermoplastic Polyurethane
Processing
Dosage: 1- 5 %
Chemical structure
Aromatic
Form of delivery
Granules
Processing conditions
Max.: 205°C
Polymer
Thermoplastic Polyurethane
Processing
Dosage: 1- 5 %
Chemical structure
Aromatic
Form of delivery
Granules
Processing conditions
Max.: 205°C
DANCOLOR TPU
Colour Masterbatches (aliphatic TPU matrix)
Product name
Description
Data sheet
Safety data sheet
Polymer
Thermoplastic polyurethane
Processing
Dosage: 1,5- 3 %
Chemical structure
Aliphatic
Form of delivery
Granules
Processing conditions
Max.: 190°C
Polymer
Thermoplastic polyurethane
Processing
Dosage: 3-5 %
Chemical structure
Aliphatic
Form of delivery
Granules
Processing conditions
Max.: 190°C
Polymer
Thermoplastic polyurethane
Processing
Dosage: 2-3 %
Chemical structure
Aliphatic
Form of delivery
Granules
Processing conditions
Max.: 240°C